Polymer Property : Decomposition Temperature = 434 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 434 °C
813 °F
Degradation Temperature
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy
A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding...