Thermal Properties Metric English Comments
Decomposition Temperature 451 °C
844 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..