Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 470 °C | 878 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos.. |
|||
Decomposition Temperature | 470 °C | 878 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A.. |