Polymer Property : Decomposition Temperature = 500 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 400 - 500 °C
752 - 932 °F
ASTM E1131
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..