Polymer Property : Decomposition Temperature = 500 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 260 °C
500 °F
Thermal Stability; ASTM D3350
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin
Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid..
Decomposition Temperature 260 °C
500 °F
Hybrid Plastics POSS® MA0717 MethacrylEthyl-POSS®
POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®..