Material Notes:
Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
F20, Condition C, ASTM D1693, 100% Igepal
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 22.5 MPa
3260 psi
ASTM D638
Elongation at Break 850 %
850 %
ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
Secant; ASTM D3350
Izod Impact, Notched 3.70 J/cm
6.93 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 128 °C
262 °F
ASTM D3417
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Decomposition Temperature 260 °C
500 °F
Thermal Stability; ASTM D3350
Processing Properties Metric English Comments
Melt Temperature 195 - 225 °C
383 - 437 °F