Polymer Property : Decomposition Temperature = 530 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature <= 530 °C
<= 986 °F
Chengdu Polyster PPHA p-Hydroxybenzoic Acid Polymer
PPHA is difficult to manufacture and brittle as well as low mechanical strength, its compounds have a higher mechanical strength and can be injection moulded. It can work without oil and its perform..