Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 360 °C | 680 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
Decomposition Temperature | 360 °C | 680 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |