Thermal Properties Metric English Comments
Decomposition Temperature 392 °C
738 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy
Product Description: EPO-TEK®H20E-FC is a two-component, electrically conductive, snap curing epoxy for photovoltaic thin film module stringing, semiconductor packaging and PCB circuit assembly.Adv..