Flame Spread 26.0 - 35.0 mm/min
1.02 - 1.38 in/min
Average value: 27.9 mm/min Grade Count:8
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..