Polymer Property : Flame Spread = 26.0 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 26.0 - 35.0 mm/min
1.02 - 1.38 in/min
Average value: 27.9 mm/min Grade Count:8
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Flame Spread 26.0 mm/min

@Thickness 3.17 mm
1.02 in/min

@Thickness 0.125 in
FH3
LG Chemical 25SPE GPPS
Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr..
Flame Spread 26.0 mm/min

@Thickness 3.17 mm
1.02 in/min

@Thickness 0.125 in
FH3
LG Chemical 25SPI GPPS
High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup..
Flame Spread 26.0 mm/min

@Thickness 3.17 mm
1.02 in/min

@Thickness 0.125 in
FH3
LG Chemical 25SPR GPPS
Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion..