Thermal Properties Metric English Comments
Flame Spread 13 mm/min
0.52 in/min
FM VSS-302
Multibase Multi-Flex® D 5308 X Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flame Spread <= 13 mm/min
<= 0.50 in/min
FM VSS-302
Multibase Multi-Flex® TEA 1004 TPO Thermoplastic Polyolefin Elastomer
Features: Adhesion, GoodPaintableWeather Resistance, Good Forms:PelletsUses: Automotive ApplicationsSealsToothbrush HandlesInformation provided by Multibase
Flame Spread 13 mm/min

@Thickness 1.00 mm
0.51 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Flame Spread 13 mm/min
0.51 in/min
FMVSS 302
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Flame Spread 13 mm/min
0.50 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS
Information provided by Asahi Thermofil