Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 23 mm/min | 0.90 in/min | FM VSS-302 |
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flame Spread | 23 mm/min @Thickness 3.00 mm |
0.91 in/min @Thickness 0.118 in |
FMVSS 302; DIN 75200 |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Flame Spread | 23 mm/min | 0.91 in/min | ASTM D635 |
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Flame Spread | 23 mm/min @Thickness 1.00 mm |
0.91 in/min @Thickness 0.0394 in |
SE/B; ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Minlon® 22C BK086 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance.. |
|||
Flame Spread | 23 mm/min | 0.90 in/min | Horizontal Burn Rate; FMVSS302 |
Asahi Kasei Thermofil P-9900-0712 Unfilled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flame Spread | 23 mm/min | 0.90 in/min | Horizontal Burn Rate; FMVSS302 |
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Flame Spread | 23 mm/min | 0.90 in/min | Horizontal Burn Rate; FMVSS302 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Flame Spread | 23 mm/min | 0.90 in/min | Horizontal Burn Rate; FMVSS302 |
Asahi Kasei Thermofil P-20TC-Y118 20% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |