Asahi Kasei Thermofil P-9900-0712 Unfilled, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P-9900-0712 Unfilled, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 17 g/10 min
17 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Yield 35 %
35 %
ASTM D638
Flexural Strength 52.4 MPa
7600 psi
ASTM D790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Flame Spread 23 mm/min
0.90 in/min
Horizontal Burn Rate; FMVSS302