Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 50.0 mm/min @Thickness 1.00 mm |
1.97 in/min @Thickness 0.0394 in |
FMVSS 302 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |