Thermal Properties Metric English Comments
CTE, linear -10.0 - 15.0 µm/m-°C
-5.56 - 8.33 µin/in-°F
Average value: 5.52 µm/m-°C Grade Count:15
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..