Polymer Property : CTE, linear = 8.33 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 15.0 - 15.0 µm/m-°C

@Temperature 55.0 - 160 °C
8.33 - 8.33 µin/in-°F

@Temperature 131 - 320 °F
Average value: 15.0 µm/m-°C Grade Count:1
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
CTE, linear 12.0 - 15.0 µm/m-°C

@Temperature -40.0 - 125 °C
6.67 - 8.33 µin/in-°F

@Temperature -40.0 - 257 °F
IPC-TM-650.2.4.41
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg
The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for..
CTE, linear 2.00 - 15.0 µm/m-°C
1.11 - 8.33 µin/in-°F
Average value: 4.82 µm/m-°C Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear -10.0 - 15.0 µm/m-°C
-5.56 - 8.33 µin/in-°F
Average value: 5.52 µm/m-°C Grade Count:15
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
CTE, linear 12.0 - 15.0 µm/m-°C

@Temperature 1000 °C
6.67 - 8.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories HAL-SNA Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).