Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.130 µm/m-°C | 0.0722 µin/in-°F | ASTM D696 |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
CTE, linear | 0.130 - 80.0 µm/m-°C | 0.0722 - 44.4 µin/in-°F | Average value: 11.2 µm/m-°C Grade Count:11 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |