Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® CH6310 PC+ABS (Asia Pacific) CH6310 is a high heat, high flow PC/ABS resin, with nonbrominated, nonchlorinated flame retardant system. All color available. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific) |
|||
CTE, linear | 71.0 - 80.0 µm/m-°C | 39.4 - 44.4 µin/in-°F | Average value: 72.5 µm/m-°C Grade Count:6 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Average value: 71.7 µm/m-°C Grade Count:3 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 63.0 - 80.0 µm/m-°C | 35.0 - 44.4 µin/in-°F | Average value: 68.7 µm/m-°C Grade Count:3 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
CTE, linear | 18.0 - 80.0 µm/m-°C | 10.0 - 44.4 µin/in-°F | Average value: 27.3 µm/m-°C Grade Count:19 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 1.50 - 80.0 µm/m-°C | 0.833 - 44.4 µin/in-°F | Average value: 23.9 µm/m-°C Grade Count:23 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C | 38.9 - 44.4 µin/in-°F | DIN 52328 |
Isoflon PVC Polyvinyl Chloride Good mechanical propertiesThermoformableGood impact resistanceInformation provided by Isoflon. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled 80C FR-V2 |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 75.0 - 80.0 µm/m-°C @Temperature 0.000 - 80.0 °C |
41.7 - 44.4 µin/in-°F @Temperature 32.0 - 176 °F |
ASTM D696 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIN-55 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIN-72 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 80.0 µm/m-°C | 5.56 - 44.4 µin/in-°F | Average value: 57.5 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C | 38.9 - 44.4 µin/in-°F | |
Hippe PVC-U Polyvinyl Chloride Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe. |
|||
CTE, linear | 3.30 - 80.0 µm/m-°C | 1.83 - 44.4 µin/in-°F | Average value: 31.4 µm/m-°C Grade Count:59 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |