Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.10 - 3.30 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.17 - 1.83 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
CTE, linear | 2.10 µm/m-°C @Temperature 20.0 °C |
1.17 µin/in-°F @Temperature 68.0 °F |
Longitudinal |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
CTE, linear | 2.10 µm/m-°C @Temperature 1000 °C |
1.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CRAG-L42 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 2.10 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
1.17 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |