Polymer Property : CTE, linear = 10.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 °C
5.72 µin/in-°F

@Temperature 68.0 °F
MarkeTech Silicon Carbide (6H) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 3.5%.
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 °C
5.72 µin/in-°F

@Temperature 68.0 °F
MarkeTech Strontium Titanate (SrTiO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 °C
5.72 µin/in-°F

@Temperature 68.0 °F
MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 600 °C
5.72 µin/in-°F

@Temperature 77.0 - 1110 °F
ICE ZrO
Data provided by the manufacturer, International Ceramic Engineering.
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 - 100 °C
5.72 µin/in-°F

@Temperature 68.0 - 212 °F
Misumi G-STAR Martensite Free-cutting Stainless Steel
Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation.
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 - 100 °C
5.72 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NIMONIC® Alloy 263
A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an..
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 °C
5.72 µin/in-°F

@Temperature 68.0 °F
Sapco Partially Stabilized TZP Zirconia (YSZ)
Information provided by Sapco.
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 1000 °C
5.72 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 1000 °C
5.72 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 10.3 µm/m-°C
5.72 µin/in-°F
Anderman Ceramics EZY 94 Zirconia, 94%, Yttria-Stabilized
Dense impervious zirconia for high wear and aggressive engineering applications. Available in many shapes and sizes.Information provided by Anderman Ceramics.
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 1000 °C
5.72 µin/in-°F

@Temperature 77.0 - 1830 °F
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide
General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use..
CTE, linear 10.3 µm/m-°C
5.72 µin/in-°F
Mateck YSZ
Substrate bicrystals for superconductivity
Copyright © lookpolymers.com All Rights Reserved