Astro Met AmZirOx 86 Zirconia - Zirconium Oxide

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Astro Met Inc.
Trade Name AmZirOx
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Astro Met AmZirOx 86 Zirconia - Zirconium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use in severe structural applications which exhibit wear, corrosion, abrasion and impact. This material is also commonly referred to as Y-TZP or Yttria Tetragonal Zirconia Polycrystal. AmZirOx 86 zirconia has been developed with a unique micro structure utilizing transformation toughening which allows AmZirOx 86 zirconia to absorb the energy of impacts that would cause most ceramics to fail.
Physical Properties Metric English Comments
Bulk Density 6.01 g/cc
0.217 lb/in³
Water Absorption 0.00 %
0.00 %
Particle Size 0.50 µm
0.50 µm
Mechanical Properties Metric English Comments
Hardness, Vickers 1290
1290
Modulus of Elasticity 204 GPa
29600 ksi
Flexural Strength 1000 MPa
145000 psi
Poissons Ratio 0.31
0.31
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
Shear Modulus 77.8 GPa
11300 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 1000 °C
5.72 µin/in-°F

@Temperature 77.0 - 1830 °F
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Thermal Conductivity 2.16 W/m-K
15.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 2400 °C
4350 °F
no load
Component Elements Properties Metric English Comments
Y2O3 5.0 %
5.0 %
ZrO2 95 %
95 %
Descriptive Properties Value Comments
Color Ivory
Gas Permeation, % 0