Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 180 µm/m-°C @Temperature -40.0 - 149 °C |
100 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
CTE, linear | 180 µm/m-°C @Temperature 23.0 - 100 °C |
100 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 23.0 - 100 °C |
100 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |
|||
CTE, linear | 180 - 180 µm/m-°C @Temperature 50.0 - 160 °C |
100 - 100 µin/in-°F @Temperature 122 - 320 °F |
Average value: 180 µm/m-°C Grade Count:1 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
|
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | ASTM D696 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | ASTM D696 |
IPB Bicell® Cellular Polypropylene Sheet Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe.. |
|||
CTE, linear | 180 µm/m-°C @Temperature -30.0 - 30.0 °C |
100 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 342-3.5 Room Temperature Cure Epoxy Adhesive TRA-BOND 342-3.5 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials such .. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 - 160 °C |
100 µin/in-°F @Temperature 68.0 - 320 °F |
Silicone Property; ASTM E 831 |
Arlon CP-499CA Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; JMTP P200 |
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 - 70.0 °C |
100 µin/in-°F @Temperature 68.0 - 158 °F |
|
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
Cured property; ASTM E831-86 |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |
|||
CTE, linear | 180 - 230 µm/m-°C | 100 - 128 µin/in-°F | Average value: 218 µm/m-°C Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 180 - 230 µm/m-°C | 100 - 128 µin/in-°F | Average value: 218 µm/m-°C Grade Count:8 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
CTE, linear | 180 µm/m-°C @Temperature -30.0 - 30.0 °C |
100 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
CTE, linear | 180 - 230 µm/m-°C | 100 - 128 µin/in-°F | Average value: 206 µm/m-°C Grade Count:17 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty.. |