CTE, linear 187 µm/m-°C
104 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy
Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid..
CTE, linear 187 - 200 µm/m-°C
104 - 111 µin/in-°F
Average value: 192 µm/m-°C Grade Count:5
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..