Material Notes:
Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
1.20 g/cc
1.20 g/cc
Part A
Viscosity 24000 - 42000 cP

@Temperature 23.0 °C
24000 - 42000 cP

@Temperature 73.4 °F
2.5 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
Tensile Modulus 1.82 GPa
263 ksi
Storage
Shear Strength 10.8 MPa
1570 psi
Lap
>= 23.4 MPa
>= 3400 psi
Die
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
Below Tg
187 µm/m-°C
104 µin/in-°F
Above Tg
Maximum Service Temperature, Air 225 °C
437 °F
Continuous
325 °C
617 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 140 °C
>= 284 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 443 °C
829 °F
Degradation Temperature
Optical Properties Metric English Comments
Refractive Index 1.5728

@Wavelength 589 nm
1.5728

@Wavelength 589 nm
Transmission, Visible 69 %

@Wavelength 600 nm
69 %

@Wavelength 600 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity >= 2.00e+12 ohm-cm
>= 2.00e+12 ohm-cm
Dielectric Constant 2.83

@Frequency 1000 Hz
2.83

@Frequency 1000 Hz
Dissipation Factor 0.011

@Frequency 1000 Hz
0.011

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 150 °C
0.0833 hour

@Temperature 302 °F
minimum
15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
minimum
30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
minimum
Pot Life 240 min
240 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Part B
Cloudy
Part A
Consistency Pourable paste
Mix Ratio By Weight 20:1
Number of Components Two
Weight Loss <0.05%
200°C
<0.05%
250°C
<0.05%
300°C