Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
CTE, linear | 175 - 225 µm/m-°C @Temperature 20.0 °C |
97.2 - 125 µin/in-°F @Temperature 68.0 °F |
|
Quadrant EPP Cestlite™ ASTL Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |