Thermal Properties Metric English Comments
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cesticolor™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestidur™ Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestilene™ HD 1000 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
CTE, linear 175 - 225 µm/m-°C

@Temperature 20.0 °C
97.2 - 125 µin/in-°F

@Temperature 68.0 °F
Quadrant EPP Cestlite™ ASTL Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.