Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.6 µm/m-°C @Temperature 25.0 - 500 °C |
9.22 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Porta Aurium 2 PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.20 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 0.000 - 100 °C |
9.20 µin/in-°F @Temperature 32.0 - 212 °F |
|
Carlson 317L 4 Austenitic Stainless Steel General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 0.000 - 100 °C |
9.20 µin/in-°F @Temperature 32.0 - 212 °F |
|
Carlson 317L 4N Austenitic Stainless Steel General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a.. |
|||
CTE, linear | 16.6 µm/m-°C @Temperature 0.000 - 100 °C |
9.20 µin/in-°F @Temperature 32.0 - 212 °F |
|
Carlson 317L Austenitic Stainless Steel Carlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel and molybdenum prese.. |