Material Notes:
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap terminals.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T <= 72
<= 72
Thickness > 0.020 Inch
Tensile Strength, Ultimate 379 - 517 MPa
55000 - 75000 psi
Tensile Strength, Yield <= 500 MPa
<= 73000 psi
0.2% offset
Elongation at Break >= 5.0 %
>= 5.0 %
in 2 in.
Tensile Modulus 138 GPa
20000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.6 µm/m-°C

@Temperature 20.0 - 300 °C
9.20 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 53.6 W/m-K
372 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 88.2 %
88.2 %
Nickel, Ni 9.5 %
9.5 %
Tin, Sn 2.3 %
2.3 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000162 ohm-cm
0.0000162 ohm-cm
Annealed