Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 °C
9.30 µin/in-°F

@Temperature 68.0 °F
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy
moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12” and in rounds up t..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.30 µin/in-°F

@Temperature 68.0 - 392 °F
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.30 µin/in-°F

@Temperature 68.0 - 392 °F
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 200 °C
9.30 µin/in-°F

@Temperature 68.0 - 392 °F
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, 1/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, Annealed
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, Extra Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, Extra Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 770 Nickel Silver 18%, Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..