Material Notes:
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connectors, sockets, clips and springs.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 579 MPa
>= 84000 psi
Tensile Strength, Yield >= 510 MPa
>= 74000 psi
0.2% offset
Elongation at Break >= 6.0 %
>= 6.0 %
in 2 in.
Tensile Modulus 128 GPa
18500 ksi
Thermal Properties Metric English Comments
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 - 300 °C
9.30 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 257.7 W/m-K
1788 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 98.5 %
98.5 %
Nickel, Ni 1.6 %
1.6 %
Silicon, Si 0.20 %
0.20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000297 ohm-cm
0.00000297 ohm-cm
Annealed