CTE, linear 27.0 - 31.0 µm/m-°C
15.0 - 17.2 µin/in-°F
Average value: 28.5 µm/m-°C Grade Count:4
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..
CTE, linear 20.0 - 31.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 - 17.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific)
50% filled FR high modulus PPE/PS blend