Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.3 µm/m-°C | 10.7 µin/in-°F | ASTM E831 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |