Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.6 µm/m-°C | 10.9 µin/in-°F | After Sintering |
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package.. |