Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 220 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 220 µm/m-°C

@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
122 µin/in-°F

@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
NeXolve Essar™ Stretch 255 Polyimide
High temperature colorless elastic polyimide. NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single ..
CTE, linear 220 µm/m-°C

@Temperature 20.0 °C
122 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White
RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DEBT (deputy tin deflagrate) as the stan..
CTE, linear 220 µm/m-°C

@Temperature 20.0 °C
122 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
CTE, linear 220 - 240 µm/m-°C
122 - 133 µin/in-°F
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no..
CTE, linear 220 µm/m-°C

@Temperature 30.0 - 150 °C
122 µin/in-°F

@Temperature 86.0 - 302 °F
Silicone Property; ASTM E 831
Arlon CP-RC-3916 Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..