Polymer Property : CTE, linear = 240 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 220 - 240 µm/m-°C
122 - 133 µin/in-°F
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no..
CTE, linear 100 - 240 µm/m-°C
55.6 - 133 µin/in-°F
Average value: 182 µm/m-°C Grade Count:26
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..