Thermal Properties Metric English Comments
CTE, linear 90.0 - 234 µm/m-°C
50.0 - 130 µin/in-°F
Average value: 128 µm/m-°C Grade Count:5
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..