Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acetal Copolymer, Silicone Filled

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Silicone Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acetal Copolymer, Silicone Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.29 - 1.62 g/cc
0.0466 - 0.0585 lb/in³
Average value: 1.41 g/cc Grade Count:17
Filler Content 2.00 - 4.00 %
2.00 - 4.00 %
Average value: 2.40 % Grade Count:5
Water Absorption 0.0500 - 0.270 %
0.0500 - 0.270 %
Average value: 0.185 % Grade Count:6
Linear Mold Shrinkage 0.00400 - 0.0350 cm/cm
0.00400 - 0.0350 in/in
Average value: 0.0215 cm/cm Grade Count:15
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0198 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79.0 - 82.0
79.0 - 82.0
Average value: 80.0 Grade Count:3
Tensile Strength, Ultimate 38.0 - 110 MPa
5510 - 16000 psi
Average value: 54.5 MPa Grade Count:12
Tensile Strength, Yield 39.0 - 62.0 MPa
5660 - 8990 psi
Average value: 49.7 MPa Grade Count:6
Elongation at Break 2.50 - 90.0 %
2.50 - 90.0 %
Average value: 25.1 % Grade Count:14
Elongation at Yield 6.00 - 24.8 %
6.00 - 24.8 %
Average value: 14.2 % Grade Count:4
Modulus of Elasticity 2.07 - 3.21 GPa
300 - 466 ksi
Average value: 2.60 GPa Grade Count:10
Flexural Yield Strength 48.0 - 172 MPa
6960 - 24900 psi
Average value: 76.4 MPa Grade Count:15
Flexural Modulus 1.70 - 7.60 GPa
247 - 1100 ksi
Average value: 2.66 GPa Grade Count:15
Izod Impact, Notched 0.440 - 0.961 J/cm
0.824 - 1.80 ft-lb/in
Average value: 0.714 J/cm Grade Count:13
0.500 - 0.500 J/cm

@Temperature -29.0 - -29.0 °C
0.937 - 0.937 ft-lb/in

@Temperature -20.2 - -20.2 °F
Average value: 0.500 J/cm Grade Count:1
Izod Impact, Unnotched 11.7 - 5340 J/cm
22.0 - 10000 ft-lb/in
Average value: 13.4 J/cm Grade Count:7
Izod Impact, Notched (ISO) 6.00 - 9.00 kJ/m²
2.86 - 4.28 ft-lb/in²
Average value: 7.00 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 52.0 - 83.0 kJ/m²
24.7 - 39.5 ft-lb/in²
Average value: 62.3 kJ/m² Grade Count:3
Coefficient of Friction 0.200 - 0.410
0.200 - 0.410
Average value: 0.270 Grade Count:3
Coefficient of Friction, Static 0.100 - 0.300
0.100 - 0.300
Average value: 0.167 Grade Count:3
K (wear) Factor 2.01 - 220 x 10-8 mm³/N-M
1.00 - 109 x 10-10 in³-min/ft-lb-hr
Average value: 74.5 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 90.0 - 234 µm/m-°C
50.0 - 130 µin/in-°F
Average value: 128 µm/m-°C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 152 - 166 °C
305 - 331 °F
Average value: 161 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 145 °C
160 - 293 °F
Average value: 102 °C Grade Count:14
Flammability, UL94 HB
HB
Grade Count:10
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm
1.00e+14 - 1.00e+16 ohm-cm
Average value: 4.42e+15 ohm-cm Grade Count:5
Dielectric Strength 17.7 - 19.7 kV/mm
450 - 500 kV/in
Average value: 18.2 kV/mm Grade Count:4
Processing Properties Metric English Comments
Melt Temperature 182 - 230 °C
360 - 446 °F
Average value: 202 °C Grade Count:8
Mold Temperature 48.9 - 120 °C
120 - 248 °F
Average value: 89.4 °C Grade Count:8
Drying Temperature 82.2 - 121 °C
180 - 250 °F
Average value: 116 °C Grade Count:7
Moisture Content 0.150 %
0.150 %
Average value: 0.150 % Grade Count:6
Dew Point -31.7 °C
-25.0 °F
Average value: -31.7 °C Grade Count:6
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:6
Users viewing this material also viewed the following: