CTE, linear 241 µm/m-°C
134 µin/in-°F
Above Tg
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive
TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t..