CTE, linear 28.0 - 28.0 µm/m-°C

@Temperature 140 - 180 °C
15.6 - 15.6 µin/in-°F

@Temperature 284 - 356 °F
Average value: 28.0 µm/m-°C Grade Count:1
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..