CTE, linear 5.10 - 5.50 µm/m-°C

@Temperature 20.0 - 450 °C
2.83 - 3.06 µin/in-°F

@Temperature 68.0 - 842 °F
Kinetics MIM F15 (Kovarâ„¢) Low CTE Alloy
High nickel, high cobalt iron alloy. A traditional metal-to- glass sealing alloy that offers a low coefficient of thermal expansion (CTE) similar to glass. Provides the hermeticity required for firm..
CTE, linear 5.00 - 5.50 µm/m-°C

@Temperature 25.0 - 800 °C
2.78 - 3.06 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories 75 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..