Material Notes:
High nickel, high cobalt iron alloy. A traditional metal-to- glass sealing alloy that offers a low coefficient of thermal expansion (CTE) similar to glass. Provides the hermeticity required for firmly bonding between metal and glass. Frequently used for hermetic enclosures or packages used to protect electronic or optical devices in aerospace, automotive, optical, optoelectronic, and telecommunication industries.Property values reported are typical for Kinetics' MIM products.Metal Injection Molding General Notes: Fine metal powders (generally
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 64.1
64.1
Tensile Strength, Ultimate 427 MPa
62000 psi
Tensile Strength, Yield 276 MPa
40000 psi
Elongation at Break 30 %
30 %
in 1 inch
Charpy Impact, Unnotched 102 J
75.0 ft-lb
1/2 size bar
Thermal Properties Metric English Comments
CTE, linear 5.10 - 5.50 µm/m-°C

@Temperature 20.0 - 450 °C
2.83 - 3.06 µin/in-°F

@Temperature 68.0 - 842 °F
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Cobalt, Co 17 %
17 %
Iron, Fe 54 %
54 %
by difference
Nickel, Ni 29 %
29 %
Descriptive Properties Value Comments
Surface Finish 32 Ra