Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 3.30 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 3.30 µm/m-°C
1.83 µin/in-°F
at Set Pt.; Crystallized
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a..
CTE, linear 3.30 µm/m-°C

@Temperature 260 °C
1.83 µin/in-°F

@Temperature 500 °F
Fired Thermal Expansion
Ferro EG 2805 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott DURAN® Borosilicate Glass
Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, general-purpose glass for apparatus for the chemical industry, for pipelines, and glasswareInformation provided by..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott DURATAN® Borosilicate Glass
Prestressed borosilicate glass 3.3, chemically and thermally highly resistant, Flameproof lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below ..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8347 Borosilicate Glass
Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, highly UV-transmitting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium i..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott KIMAX® Borosilicate Glass
Laboratory Glass Drainline from Borosilicate glass 3.3. Chemically and thermally highly resistant.The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott BORO-8330â„¢ Borosilicate Glass
Borosilicate glass 3.3 acc. ISO 3585, chemically highly resistant, highly resistant to thermal shock, special applications in the pharmaceutical industryInformation provided by SCHOTT AG.
CTE, linear 3.30 µm/m-°C

@Temperature 25.0 - 1000 °C
1.83 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 3.30 µm/m-°C
1.83 µin/in-°F
Esstech V-124-1110 Strontium Borosilicate Glass
Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-4.Information provided by ESSTECH, Inc.
CTE, linear 3.30 µm/m-°C
1.83 µin/in-°F
Esstech V-124-1125 Strontium Borosilicate Glass
Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-3.Information provided by ESSTECH, Inc.
CTE, linear 3.30 µm/m-°C

@Temperature 1000 °C
1.83 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CRAG-L44 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 3.30 - 80.0 µm/m-°C
1.83 - 44.4 µin/in-°F
Average value: 31.4 µm/m-°C Grade Count:59
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 300 °C
1.83 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott CONTURAX® Borosilicate Glass
Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi..