Thermal Properties Metric English Comments
CTE, linear 6.20 µm/m-°C
3.44 µin/in-°F
Plansee Chromium, Cr; Sintered
Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess..
CTE, linear 6.20 µm/m-°C
3.44 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro CF 7586 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..
CTE, linear 6.20 µm/m-°C
3.44 µin/in-°F
at Set Pt.
Ferro EG 2782 Specialty Glass
Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase..
CTE, linear 6.20 µm/m-°C

@Temperature 260 °C
3.44 µin/in-°F

@Temperature 500 °F
Ferro EG 2782 Specialty Glass
Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase..
CTE, linear 6.20 - 6.60 µm/m-°C

@Temperature 20.0 - 100 °C
3.44 - 3.67 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 1100 °C
3.44 µin/in-°F

@Temperature 68.0 - 2010 °F
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.
CTE, linear 6.20 µm/m-°C

@Temperature 25.0 - 100 °C
3.44 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite
High stiffness, low density, low CTE composite. Components can be formed with complicated features, and can be machined to tight tolerances. Applications in high-precision equipment--semiconductor..
CTE, linear 6.20 µm/m-°C

@Temperature 20.0 - 1000 °C
3.44 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 1370DP Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company
CTE, linear 6.20 - 7.60 µm/m-°C

@Temperature 25.0 - 800 °C
3.44 - 4.22 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods
LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat..
Copyright © lookpolymers.com All Rights Reserved