Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.20 µm/m-°C | 3.44 µin/in-°F | |
Plansee Chromium, Cr; Sintered Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess.. |
|||
CTE, linear | 6.20 µm/m-°C | 3.44 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro CF 7586 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t.. |
|||
CTE, linear | 6.20 µm/m-°C | 3.44 µin/in-°F | at Set Pt. |
Ferro EG 2782 Specialty Glass Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase.. |
|||
CTE, linear | 6.20 µm/m-°C @Temperature 260 °C |
3.44 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2782 Specialty Glass Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase.. |
|||
CTE, linear | 6.20 - 6.60 µm/m-°C @Temperature 20.0 - 100 °C |
3.44 - 3.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
CTE, linear | 6.20 µm/m-°C @Temperature 20.0 - 1100 °C |
3.44 µin/in-°F @Temperature 68.0 - 2010 °F |
|
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |
|||
CTE, linear | 6.20 µm/m-°C @Temperature 25.0 - 100 °C |
3.44 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite High stiffness, low density, low CTE composite. Components can be formed with complicated features, and can be machined to tight tolerances. Applications in high-precision equipment--semiconductor.. |
|||
CTE, linear | 6.20 µm/m-°C @Temperature 20.0 - 1000 °C |
3.44 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ceralloy® 1370DP Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company |
|||
CTE, linear | 6.20 - 7.60 µm/m-°C @Temperature 25.0 - 800 °C |
3.44 - 4.22 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |