Thermal Properties Metric English Comments
CTE, linear 3.50 µm/m-°C

@Temperature 23.0 - 260 °C
1.94 µin/in-°F

@Temperature 73.4 - 500 °F
ASTM D696
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L
CTE, linear 3.50 µm/m-°C
1.94 µin/in-°F
at Set Pt.
Ferro EG 2790 Metal Sealing
Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,..
CTE, linear 3.50 µm/m-°C

@Temperature 260 °C
1.94 µin/in-°F

@Temperature 500 °F
Ferro EG 2790 Metal Sealing
Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,..
CTE, linear 3.50 µm/m-°C

@Temperature 25.0 - 1000 °C
1.94 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide
Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 3.50 µm/m-°C

@Temperature 1000 °C
1.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BTCQ Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 3.50 µm/m-°C

@Temperature 1000 °C
1.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SBSN20 Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 3.50 µm/m-°C

@Temperature 25.0 - 500 °C
1.94 µin/in-°F

@Temperature 77.0 - 932 °F
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber
Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus..
CTE, linear 3.50 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.94 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
CTE, linear 3.50 µm/m-°C

@Temperature 20.0 - 500 °C
1.94 µin/in-°F

@Temperature 68.0 - 932 °F
Zircar Ceramics ASH Alumina-Silica Insulation
ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its..