CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide

Category Ceramic , Carbide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Data Provided by the manufacturer, CoorsTek, Inc.
Physical Properties Metric English Comments
Density 2.90 g/cc
0.105 lb/in³
ASTM C20
Water Absorption 0.00 %
0.00 %
ASTM 373
Particle Size 12 µm
12 µm
Thin Section Crystal Size
Mechanical Properties Metric English Comments
Knoop Microhardness 23
23
1000 g
Modulus of Elasticity 150 GPa
21800 ksi
ASTM C848
Flexural Strength 90.0 MPa
13100 psi
ASTM F417
Poissons Ratio 0.20
0.20
ASTM C848
Fracture Toughness 2.90 MPa-m½
2.64 ksi-in½
Notched Beam
Shear Modulus 63.0 GPa
9140 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.50 µm/m-°C

@Temperature 25.0 - 1000 °C
1.94 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1000 °C
1830 °F
No Load
Descriptive Properties Value Comments
Color Black