Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.0 - 57.6 µm/m-°C | 12.8 - 32.0 µin/in-°F | Average value: 43.9 µm/m-°C Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
CTE, linear | 19.8 - 57.6 µm/m-°C | 11.0 - 32.0 µin/in-°F | Average value: 38.2 µm/m-°C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
CTE, linear | 19.8 - 57.6 µm/m-°C | 11.0 - 32.0 µin/in-°F | Average value: 35.6 µm/m-°C Grade Count:5 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 12.0 - 57.6 µm/m-°C | 6.67 - 32.0 µin/in-°F | Average value: 18.2 µm/m-°C Grade Count:42 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |