Thermal Properties Metric English Comments
CTE, linear 19.8 - 30.1 µm/m-°C

@Temperature 20.0 °C
11.0 - 16.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Network Polymers Kepital® F20-25
Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc.
CTE, linear 19.8 µm/m-°C

@Temperature -40.0 - 150 °C
11.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet)
CTE, linear 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Quantum PEEK 30% Carbon Filled
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 19.8 - 139 µm/m-°C
11.0 - 77.2 µin/in-°F
Average value: 72.2 µm/m-°C Grade Count:46
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
CTE, linear 19.8 µm/m-°C

@Temperature -40.0 - 149 °C
11.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
CTE, linear 19.8 - 54.0 µm/m-°C
11.0 - 30.0 µin/in-°F
Average value: 32.9 µm/m-°C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
CTE, linear 19.8 - 57.6 µm/m-°C
11.0 - 32.0 µin/in-°F
Average value: 38.2 µm/m-°C Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
CTE, linear 19.8 - 57.6 µm/m-°C
11.0 - 32.0 µin/in-°F
Average value: 35.6 µm/m-°C Grade Count:5
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
CTE, linear 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced  (discontinued **)
Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom..
CTE, linear 19.8 - 180 µm/m-°C
11.0 - 100 µin/in-°F
Average value: 68.4 µm/m-°C Grade Count:29
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
CTE, linear 19.8 - 41.4 µm/m-°C
11.0 - 23.0 µin/in-°F
Average value: 27.0 µm/m-°C Grade Count:9
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
CTE, linear 19.8 µm/m-°C
11.0 µin/in-°F
Average value: 19.8 µm/m-°C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
CTE, linear 19.8 - 55.8 µm/m-°C
11.0 - 31.0 µin/in-°F
Average value: 34.2 µm/m-°C Grade Count:29
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
CTE, linear 19.8 - 30.0 µm/m-°C
11.0 - 16.7 µin/in-°F
Average value: 22.5 µm/m-°C Grade Count:5
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear 19.8 - 400 µm/m-°C
11.0 - 222 µin/in-°F
Average value: 73.1 µm/m-°C Grade Count:13
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
CTE, linear 19.8 µm/m-°C

@Temperature 22.8 - 260 °C
11.0 µin/in-°F

@Temperature 73.0 - 500 °F
ASTM E831
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide
Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® ..
CTE, linear 19.8 µm/m-°C

@Temperature 20.0 °C
11.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tempalux® 30% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
CTE, linear 19.8 - 170 µm/m-°C
11.0 - 94.4 µin/in-°F
Average value: 88.1 µm/m-°C Grade Count:36
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 19.8 µm/m-°C

@Temperature 20.0 °C
11.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Quantum PEI - Ultem® 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 19.8 µm/m-°C

@Temperature 20.0 °C
11.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.