Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
modified; ASTM D696 |
Solvay Engineered Polymers DEXFLEX® 711-300 TPO
(discontinued **) Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color match.. |
|||
CTE, linear | 71.0 - 80.0 µm/m-°C | 39.4 - 44.4 µin/in-°F | Average value: 72.5 µm/m-°C Grade Count:6 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG902 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG902L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMG314V Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMG334V Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMH454 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® Rapide CLG 356B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1340 Crystal Polystyrene 1340 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades such as LACQRENE® 7240. In dilution, LACQRENE® 1340 gives excellent pro.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM D696 |
Total PSC 1450 High Heat Resistance, Easy Flow Crystal Polystyrene Total Petrochemicals Polystyrene 1450 is a high heat resistance, easy flow crystal polystyrene for injection molding and the foam extrusion industry. This product offers optimum fluidity and excell.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG357 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |